# Lithium-metal anodes: dendrites, the SEI and four ways to stop them

> Why the lithium-metal anode, with 3,860 mAh g⁻¹ at −3.040 V vs SHE, is hard to cycle: each plating–stripping cycle cracks and re-forms the SEI, grows dendrites and strands isolated metallic lithium, which titration gas chromatography shows is the main inactive lithium. Four fixes follow with their numbers: an FEC-made LiF-rich SEI, a concentrated 4 M LiFSI–DME electrolyte, a layered reduced-graphene-oxide host and a stiff solid electrolyte, with its critical stripping current.

- Page: https://www.labcanvas.com/templates/graphical-abstracts/lithium-metal-anodes-dendrites-sei-four-ways-stop-them
- Open in the LabCanvas editor (LabCanvas account): https://www.labcanvas.com/editor.html?template=lithium-metal-anode-dendrites-sei-and-four-fixes
- Updated: 2026-10-14
- Category: Graphical abstracts
- Method: Graphical abstract
- Starting materials: A lithium-metal anode facing a cathode across a liquid or solid electrolyte
- Product: An anode that plates and strips lithium evenly, with high Coulombic efficiency and no short circuit
- Key result: 3,860 mAh g⁻¹ and −3.040 V vs SHE (Xu et al. 2014); unreacted Li⁰ dominates inactive Li (Fang et al. 2019); CE 98% with FEC (Zhang et al. 2017); CE up to 99.1%, > 6,000 cycles at 10 mA cm⁻² in 4 M LiFSI–DME (Qian et al. 2015); ~20% dimension change in a 7 wt% rGO host (Lin et al. 2016); shear modulus ≈ 2× Li (Monroe & Newman 2005); critical stripping current 0.2 mA cm⁻² at 3 MPa (Kasemchainan et al. 2019)
- Figure: 1920 × 1080 px, 85 editable layers (6 generated objects with settings)

## Steps

1. **a · The prize**: Lithium metal stores 3,860 mAh g⁻¹ at the lowest potential of any anode, −3.040 V vs SHE, but has no host lattice, so its volume changes almost without limit (Xu et al. 2014; Lin et al. 2016)
2. **b · The problem**: Plating cracks the SEI, fresh SEI forms on the exposed lithium, dendrites grow, and stripping leaves isolated Li⁰ in SEI shells; that unreacted Li⁰, not SEI Li⁺, is most of the inactive lithium (Fang et al. 2019)
3. **c · Fluorinate the SEI**: An FEC additive forms a compact, LiF-rich SEI: 98% Coulombic efficiency within 100 cycles in Li | Cu cells (Zhang et al. 2017)
4. **c · Concentrate the electrolyte**: 4 M LiFSI in DME: Coulombic efficiency up to 99.1% and Li | Li cells cycled more than 6,000 times at 10 mA cm⁻² (Qian et al. 2015)
5. **c · Give lithium a host**: 7 wt% layered reduced graphene oxide holds the lithium: about 20% dimension change and up to ~3,390 mAh g⁻¹ (Lin et al. 2016)
6. **c · Go solid**: A separator about twice as stiff in shear as lithium suppresses roughening (Monroe & Newman 2005), but stripping above 0.2 mA cm⁻² at 3 MPa leaves voids that seed dendrites in Li₆PS₅Cl cells (Kasemchainan et al. 2019)

## Uses

- Graphical abstracts on lithium-metal and anode-free batteries
- Talks on dendrites, the SEI and dead lithium
- Teaching why lithium metal is hard to cycle

## References

1. Xu, Wang, Ding, Chen, Nasybulin, Zhang & Zhang, “Lithium metal anodes for rechargeable batteries”, Energy Environ. Sci. 2014. https://doi.org/10.1039/C3EE40795K (review)
2. Fang et al., “Quantifying inactive lithium in lithium metal batteries”, Nature 2019. https://doi.org/10.1038/s41586-019-1481-z (primary)
3. Li et al., “Atomic structure of sensitive battery materials and interfaces revealed by cryo-electron microscopy”, Science 2017. https://doi.org/10.1126/science.aam6014 (primary)
4. Lin, Liu, Liang, Lee, Sun, Wang, Yan, Xie & Cui, “Layered reduced graphene oxide with nanoscale interlayer gaps as a stable host for lithium metal anodes”, Nat. Nanotechnol. 2016. https://doi.org/10.1038/nnano.2016.32 (primary)
5. Zhang, Cheng, Chen, Yan & Zhang, “Fluoroethylene carbonate additives to render uniform Li deposits in lithium metal batteries”, Adv. Funct. Mater. 2017. https://doi.org/10.1002/adfm.201605989 (primary)
6. Qian, Henderson, Xu, Bhattacharya, Engelhard, Borodin & Zhang, “High rate and stable cycling of lithium metal anode”, Nat. Commun. 2015. https://doi.org/10.1038/ncomms7362 (primary)
7. Monroe & Newman, “The impact of elastic deformation on deposition kinetics at lithium/polymer interfaces”, J. Electrochem. Soc. 2005. https://doi.org/10.1149/1.1850854 (primary)
8. Kasemchainan, Zekoll, Spencer Jolly, Ning, Hartley, Marrow & Bruce, “Critical stripping current leads to dendrite formation on plating in lithium anode solid electrolyte cells”, Nat. Mater. 2019. https://doi.org/10.1038/s41563-019-0438-9 (primary)
9. Cheng, Zhang, Zhao & Zhang, “Toward safe lithium metal anode in rechargeable batteries: a review”, Chem. Rev. 2017. https://doi.org/10.1021/acs.chemrev.7b00115 (review)

Credit: Drawn by LabCanvas after Xu et al., Energy Environ. Sci. 2014 (doi:10.1039/C3EE40795K); Fang et al., Nature 2019 (doi:10.1038/s41586-019-1481-z); Li et al., Science 2017 (doi:10.1126/science.aam6014); Lin et al., Nat. Nanotechnol. 2016 (doi:10.1038/nnano.2016.32); Zhang et al., Adv. Funct. Mater. 2017 (doi:10.1002/adfm.201605989); Qian et al., Nat. Commun. 2015 (doi:10.1038/ncomms7362); Monroe & Newman, J. Electrochem. Soc. 2005 (doi:10.1149/1.1850854); Kasemchainan et al., Nat. Mater. 2019 (doi:10.1038/s41563-019-0438-9). Cell, steps and grains schematic.

## Questions

**What does the “Lithium-metal anodes: dendrites, the SEI and four ways to stop them” template show?** Why the lithium-metal anode, with 3,860 mAh g⁻¹ at −3.040 V vs SHE, is hard to cycle: each plating–stripping cycle cracks and re-forms the SEI, grows dendrites and strands isolated metallic lithium, which titration gas chromatography shows is the main inactive lithium. Four fixes follow with their numbers: an FEC-made LiF-rich SEI, a concentrated 4 M LiFSI–DME electrolyte, a layered reduced-graphene-oxide host and a stiff solid electrolyte, with its critical stripping current.

**What are the steps shown in “Lithium-metal anodes: dendrites, the SEI and four ways to stop them”?** 1. a · The prize: Lithium metal stores 3,860 mAh g⁻¹ at the lowest potential of any anode, −3.040 V vs SHE, but has no host lattice, so its volume changes almost without limit (Xu et al. 2014; Lin et al. 2016). 2. b · The problem: Plating cracks the SEI, fresh SEI forms on the exposed lithium, dendrites grow, and stripping leaves isolated Li⁰ in SEI shells; that unreacted Li⁰, not SEI Li⁺, is most of the inactive lithium (Fang et al. 2019). 3. c · Fluorinate the SEI: An FEC additive forms a compact, LiF-rich SEI: 98% Coulombic efficiency within 100 cycles in Li | Cu cells (Zhang et al. 2017). 4. c · Concentrate the electrolyte: 4 M LiFSI in DME: Coulombic efficiency up to 99.1% and Li | Li cells cycled more than 6,000 times at 10 mA cm⁻² (Qian et al. 2015). 5. c · Give lithium a host: 7 wt% layered reduced graphene oxide holds the lithium: about 20% dimension change and up to ~3,390 mAh g⁻¹ (Lin et al. 2016). 6. c · Go solid: A separator about twice as stiff in shear as lithium suppresses roughening (Monroe & Newman 2005), but stripping above 0.2 mA cm⁻² at 3 MPa leaves voids that seed dendrites in Li₆PS₅Cl cells (Kasemchainan et al. 2019).

**What are the starting materials and the product?** Starting materials: A lithium-metal anode facing a cathode across a liquid or solid electrolyte. Product: An anode that plates and strips lithium evenly, with high Coulombic efficiency and no short circuit.

**Which papers is “Lithium-metal anodes: dendrites, the SEI and four ways to stop them” based on?** Xu, Wang, Ding, Chen, Nasybulin, Zhang & Zhang, “Lithium metal anodes for rechargeable batteries”, Energy Environ. Sci. 2014 (doi:10.1039/C3EE40795K); Fang et al., “Quantifying inactive lithium in lithium metal batteries”, Nature 2019 (doi:10.1038/s41586-019-1481-z); Li et al., “Atomic structure of sensitive battery materials and interfaces revealed by cryo-electron microscopy”, Science 2017 (doi:10.1126/science.aam6014); Lin, Liu, Liang, Lee, Sun, Wang, Yan, Xie & Cui, “Layered reduced graphene oxide with nanoscale interlayer gaps as a stable host for lithium metal anodes”, Nat. Nanotechnol. 2016 (doi:10.1038/nnano.2016.32); Zhang, Cheng, Chen, Yan & Zhang, “Fluoroethylene carbonate additives to render uniform Li deposits in lithium metal batteries”, Adv. Funct. Mater. 2017 (doi:10.1002/adfm.201605989); Qian, Henderson, Xu, Bhattacharya, Engelhard, Borodin & Zhang, “High rate and stable cycling of lithium metal anode”, Nat. Commun. 2015 (doi:10.1038/ncomms7362); Monroe & Newman, “The impact of elastic deformation on deposition kinetics at lithium/polymer interfaces”, J. Electrochem. Soc. 2005 (doi:10.1149/1.1850854); Kasemchainan, Zekoll, Spencer Jolly, Ning, Hartley, Marrow & Bruce, “Critical stripping current leads to dendrite formation on plating in lithium anode solid electrolyte cells”, Nat. Mater. 2019 (doi:10.1038/s41563-019-0438-9); Cheng, Zhang, Zhao & Zhang, “Toward safe lithium metal anode in rechargeable batteries: a review”, Chem. Rev. 2017 (doi:10.1021/acs.chemrev.7b00115).

**Can I edit the “Lithium-metal anodes: dendrites, the SEI and four ways to stop them” template?** Yes. Open it in the LabCanvas editor: all 85 layers are editable, including 6 generated objects (structures, plots, equipment) with their own settings. Change the text, colours and layout, then export PNG, TIFF or PDF at the width and DPI the journal asks for.