# Battery cycling plot: capacity retention and coulombic efficiency

> Paste cycle, charge and discharge capacity: specific capacity (mAh/g), capacity retention and coulombic efficiency plotted against cycle number. Free.

URL: https://www.labcanvas.com/tools/battery-cycling-plot

Paste the capacities per cycle from your cycler (cycle, charge capacity, discharge capacity), or its raw time–voltage–current export, enter the active-material mass, and you get specific capacity in mAh/g (capacity in mAh × 1000 / mass in mg), capacity retention (discharge capacity of each cycle / that of the reference cycle) and coulombic efficiency (discharge / charge, or charge / discharge for an anode half-cell) for every cycle, plotted against cycle number on two axes, with the first-cycle loss, the mean CE and the cycles to 80 % retention.

## Quick answer

- **What it does:** Plots specific capacity and coulombic efficiency against cycle number from a cycler’s per-cycle capacities (or its raw data), with capacity retention, first-cycle CE and loss, mean CE and cycles to 80 %.
- **Formula:** specific capacity (mAh/g) = Q (mAh) × 1000 / m (mg); retention = Q_dis,n / Q_dis,ref; CE = Q_dis / Q_ch (cathode, full cell) or Q_ch / Q_dis (anode half-cell)
- **Example:** The built-in graphite‖NMC coin cell (15 mg NMC, 100 cycles) gives 164.5 mAh/g in cycle 1 (2.467 mAh × 1000 / 15 mg) and 141.7 mAh/g in cycle 100, 86.14 % retention; first-cycle CE 88.50 % (21.38 mAh/g lost) and a mean CE of 99.883 % from cycle 3 on.

Free, in the browser, no account needed. Updated 2026-11-17.

## Features

- Paste cycle, charge and discharge capacity (mAh, Ah, µAh, or already mAh/g) with or without a header, or a raw cycler export with time, voltage, current and cycle number
- Specific capacity in mAh/g from the active-material mass
- Discharge (and charge) capacity and coulombic efficiency against cycle number on two y axes, CE values off the axis noted
- Capacity retention against the first cycle or any reference cycle (to leave out formation cycles)
- First-cycle coulombic efficiency and irreversible capacity, mean CE from cycle 3 on, cycles to 80 % retention
- Cathode or full cell (discharge / charge) and anode or Li-metal half-cell (charge / discharge)
- From raw data: capacities integrated from the current, energy efficiency, mean discharge voltage and rate-capability steps
- Copy the per-cycle table (pastes into Excel) and a methods sentence; PNG at 300 or 600 dpi; CSV

## How to use it

1. **Paste or drop your cycling data**: Three columns from the cycler’s cycle summary: cycle number, charge capacity, discharge capacity. A header tells the unit; without one, choose it. A raw export (time, voltage, current, cycle) also works.
2. **Enter the active mass and the cell type**: The active-material mass in mg gives mAh/g. Pick discharge / charge for a cathode half-cell or full cell, charge / discharge for an anode or Li||Cu half-cell. To measure retention from cycle 3, enter 3.
3. **Read the plot**: Look at the capacity fade and the CE trace; read the retention, the first-cycle CE and the mean CE.
4. **Take it further**: Copy the table, download the plot, or open your data in the LabCanvas Graph app to style it for a paper.

## At a glance

| | |
| --- | --- |
| Input | Cycle, charge and discharge capacity (mAh, Ah, µAh, mAh/g), or time, voltage, current and cycle |
| Output | Specific capacity, retention, CE per cycle; first-cycle CE and loss; mean CE; cycles to 80 % |
| Plot | Capacity and coulombic efficiency against cycle number, two axes |
| CE | Discharge / charge (cathode, full cell) or charge / discharge (anode half-cell) |
| Engine | The LabCanvas Graph app’s battery cycling analysis |

## How it works

$$q_n = \frac{Q_n\ (\mathrm{mAh}) \times 1000}{m\ (\mathrm{mg})}\ \ \mathrm{mAh\,g^{-1}}$$

$$\mathrm{retention}_n = \frac{Q_{\mathrm{dis},n}}{Q_{\mathrm{dis,ref}}}$$

$$\mathrm{CE}_n = \frac{Q_{\mathrm{out},n}}{Q_{\mathrm{in},n}}$$

**Specific capacity.** The capacity a cell delivers divided by the mass of active material in the electrode (not the whole electrode or cell), so 2.467 mAh from 15 mg of NMC is 164.5 mAh/g. Report the mass you used and whether capacities are per cathode, anode or total active mass.

**Retention.** The discharge capacity of each cycle as a fraction of a reference cycle: the first cycle by default, or a later one so the formation cycles at a lower rate are left out. “Cycles to 80 %” is the first cycle whose retention falls below 80 %, a common end-of-life criterion.

**Coulombic efficiency.** The charge taken out over the charge put in during the same cycle: discharge / charge for a cathode half-cell or a full cell, charge (stripping, delithiation) / discharge (plating, lithiation) for an anode or Li||Cu half-cell. The first cycle is low because lithium is consumed in forming the solid electrolyte interphase (Peled 1979); the mean CE is taken from cycle 3 on so formation does not drag it down. For the CEⁿ projection and the CE needed for a target cycle life, use the [Coulombic efficiency calculator](https://www.labcanvas.com/tools/coulombic-efficiency-calculator).

**From raw data.** With time, current and voltage, each half cycle’s capacity is the trapezoidal integral of |I| over time, and energy the integral of |I|·V; rests (|I| below half the cycle’s median current) are left out.

**Same numbers as the Graph app.** The page runs the LabCanvas Graph app's battery cycling analysis (checked against NumPy’s trapezoid on the same data); the hand-off opens the same table and plot there.

Sources: Peled E. *J Electrochem Soc* 1979;126:2047, [doi:10.1149/1.2128859](https://doi.org/10.1149/1.2128859). First-cycle and average CE as in the [Coulombic efficiency calculator](https://www.labcanvas.com/tools/coulombic-efficiency-calculator) (Chem Sci 2026, [doi:10.1039/d6sc04167a](https://doi.org/10.1039/d6sc04167a); iScience 2025, [doi:10.1016/j.isci.2025.114581](https://doi.org/10.1016/j.isci.2025.114581)).

## Worked example: 100 cycles of an NMC coin cell, and two published first cycles

The built-in example is synthetic, not a measurement: the capacities per cycle of a graphite‖NMC coin cell with 15 mg of NMC, two formation cycles at C/10 then 98 at C/2, as the Graph app integrates them from its raw cycling example.

- **Specific capacity.** Cycle 1 discharges 2.467 mAh: \(2.467 \times 1000 / 15 = \mathbf{164.5\ mAh\,g^{-1}}\). Cycle 100 gives 141.7 mAh/g.
- **First cycle.** Charge 185.87, discharge 164.49 mAh/g: CE = 164.49 / 185.87 = **88.50 %**, and 21.38 mAh/g is lost to the SEI.
- **Retention.** 141.7 / 164.5 = **86.14 %** after 100 cycles against cycle 1. Cycle 3 is the first at C/2 (159.1 mAh/g); entering 3 as the reference cycle gives 89.04 %, the fade at a constant rate.
- **Mean CE.** From cycle 3 on the CE averages **99.883 %**; 80 % retention is not reached within 100 cycles.

**Published first cycles.** A hard carbon half-cell with 370 mAh/g on sodiation (discharge) and 298 mAh/g on desodiation (charge) has CE = 298 / 370 = 80.5 % with charge / discharge selected (Chem Sci 2026, doi:10.1039/d6sc04167a). A full cell with 117.35 mAh/g charge and 99.94 mAh/g discharge has CE = 85.16 % with discharge / charge (iScience 2025, doi:10.1016/j.isci.2025.114581). Pasting either as cycle 1 gives those values.



## Questions

### How do I calculate specific capacity in mAh/g?

Divide the capacity in mAh by the mass of active material in grams: 2.467 mAh from 15 mg (0.015 g) is 164.5 mAh/g. Use the active material only, not the binder, carbon or current collector.

### How do I calculate capacity retention?

Divide each cycle’s discharge capacity by the discharge capacity of a reference cycle and multiply by 100. Use the first cycle, or the first cycle after formation if the formation cycles ran at a lower rate.

### How do I plot capacity and coulombic efficiency on one graph?

Put cycle number on the x axis, capacity (mAh/g) on the left y axis and coulombic efficiency (%) on the right y axis, with the CE axis zoomed to about 95–100 % so small changes show. This page draws exactly that plot from your data.

### Why is the first-cycle coulombic efficiency low?

In the first cycle lithium (or sodium) is consumed to form the solid electrolyte interphase and some is trapped in the electrode, so less charge comes back than went in. Typical graphite and NMC cells show 85–92 % in the first cycle and above 99.5 % later.

### Should CE be discharge/charge or charge/discharge?

Discharge / charge for a cathode half-cell or a full cell. For an anode half-cell (graphite, silicon or hard carbon against Li or Na) or a Li||Cu cell the first step is a discharge (lithiation or plating), so CE = charge / discharge. CE above 100 % usually means the wrong choice.

### Can I use the raw data from my cycler?

Yes. A file with time, voltage, current and cycle number (EC-Lab, or a Neware or Arbin export saved as CSV) works: the capacities are integrated from the current over time for each half cycle.